Effect of Al2O3 or MgO on liquidus line in the FeOX corner of FeOX-SiO2-CaO system at 1523 K under various oxygen partial pressures

Ohno, Hiroyuki, Henao, Hector M. and Itagaki, Kimio (2011) Effect of Al2O3 or MgO on liquidus line in the FeOX corner of FeOX-SiO2-CaO system at 1523 K under various oxygen partial pressures. High Temperature Materials and Processes, 30 4-5: 333-338. doi:10.1515/HTMP.2011.053

Attached Files (Some files may be inaccessible until you login with your UQ eSpace credentials)
Name Description MIMEType Size Downloads
UQ268989_OA.pdf Full text (open access) application/pdf 246.74KB 0

Author Ohno, Hiroyuki
Henao, Hector M.
Itagaki, Kimio
Title Effect of Al2O3 or MgO on liquidus line in the FeOX corner of FeOX-SiO2-CaO system at 1523 K under various oxygen partial pressures
Formatted title
Effect of Al2O3 or MgO on liquidus line in the FeOX corner of FeOX-SiO2-CaO system at 1523 K under various oxygen partial pressures
Journal name High Temperature Materials and Processes   Check publisher's open access policy
ISSN 0334-6455
2191-0324
Publication date 2011-08
Sub-type Article (original research)
DOI 10.1515/HTMP.2011.053
Open Access Status File (Publisher version)
Volume 30
Issue 4-5
Start page 333
End page 338
Total pages 6
Place of publication Berlin, Germany
Publisher Walter de Gruyter GmbH
Collection year 2012
Language eng
Formatted abstract
The liquidus line in the FeOX corner of FeOXSiO2-CaO system and the effect by adding Al2O3 or MgO to this plain system on the liquidus line were experimentally investigated at 1523 K in a wide range of oxygen partial pressure between about 10-12 and about 10-4 atm and for given (mass% CaO=mass% SiO2) ratios in the system between 0 and about 1. It was found for the plain system that the liquidus line remarkably shifted toward the low FeOX-content region when the partial pressure of oxygen was increased from 10-10 to 10-8 atm. It was clarified that the addition of Al2O3 made the homogeneous region wide only in a strongly reducing atmosphere while the addition of MgO made the homogeneous liquid region remarkably narrow at all the oxygen partial pressures and all the (mass% CaO=mass% SiO2/ ratios investigated in the study. 
Keyword Liquidus line
FeOx-SiO2-CaO-Al2O3 system
FeOx-SiO2-CaO-MgO system
Oxygen partial pressure
Q-Index Code C1
Q-Index Status Confirmed Code
Institutional Status UQ

Document type: Journal Article
Sub-type: Article (original research)
Collections: School of Chemical Engineering Publications
Official 2012 Collection
 
Versions
Version Filter Type
Citation counts: TR Web of Science Citation Count  Cited 0 times in Thomson Reuters Web of Science Article